For Thermal Conduction

 

 

 
FEATURES

Room temperature or heat cure
Resistance to temperature extremes
Primer-less adhesion to many substrates
Non-corrosive to metals
Excellent controlled volatility of low molecular weight
Excellent thermal conduction
UL approved

 
 
  FEATURES

Room temperature or heat cure
Resistance to temperature extremes
Primer-less adhesion to many substrates
Non-corrosive to metals
Excellent controlled volatility of low molecular weight
Excellent thermal conduction
UL approved

 

 

 
Key Properties Units

ES2031W

   Material Type            

-

Silicone

   One or Two-Part

-

One

   Curing Type

-

Room temperature

   Color

-

White

   Viscosity

cP

80000

   Specific Gravity

g/cm3

1.7

   Tack-Free Time

minutes

10

   Hardness

Shore

A 70

   Tensile Strength

MPa

2.0

   Elongation

%

50

   Shear Strength (AL)

MPa

1.5

   Thermal Conductivity

W/m.k

0.85

   Volume Resistivity

Ω.cm

1.0x1013

   Dielectric Strength

kV/mm

20

   Dielectric Constant (50Hz)

-

5

   Dielectric Loss (50Hz)

-

0.1

   Volatile Siloxane(D3~D10)

ppm

<150

   UL Flame Retardancy

-

UL 94 V-0

   Curing Time

-

25°C*7days

Key Properties Units

ES3044P

   Material Type            

-

Silicone

   One or Two-Part

-

One

   Curing Type

-

Room temperature

   Color

-

White

   Viscosity

cP

130000

   Specific Gravity

g/cm3

2.67

   Tack-Free Time

minutes

10

   Hardness

Shore

A 94

   Tensile Strength

MPa

0.5

   Elongation

%

-

   Shear Strength (AL)

MPa

0.5

   Thermal Conductivity

W/m.k

2.0

   Volume Resistivity

Ω.cm

1.0x1011

   Dielectric Strength

kV/mm

12

   Dielectric Constant (50Hz)

-

8

   Dielectric Loss (50Hz)

-

0.3

   Volatile Siloxane(D3~D10)

ppm

<300

   UL Flame Retardancy

-

UL 94 V-0

   Curing Time

-

25°C*7days

Key Properties Units

ESMH2610-G

   Material Type

-

Silicone

   One or Two-Part

-

One

   Curing Type

-

Heat curing

   Color

-

Gray

   Viscosity

cP

70000

   Specific Gravity

g/cm3

2.67

   Tack-Free Time

minutes

48

   Hardness

Shore

A 90

   Tensile Strength

MPa

2.0

   Elongation

%

30

   Shear Strength (AL)

MPa

0.8

   Thermal Conductivity

W/m.k

1.9

   Volume Resistivity

Ω.cm

1.0x1013

   Dielectric Strength

kV/mm

18

   Dielectric Constant (50Hz)

-

60

   Dielectric Loss (50Hz)

-

0.1

   Volatile Siloxane(D3~D10)

ppm

-

   UL Flame Retardancy

-

-

   Curing Time

-

150℃*30mins

For more product specifications, please contact your salesperson or agent.